Corrosión localizada del acero inoxidable austenítico en medio de cultivo celular y
evaluación de la citotoxicidad de los iones liberados
Abstract
Austenitic stainless steel ASTM F745 has been submitted to localized corrosion in cell culture medium and NaCl aqueous solution, whose chloride concentrations were 4413,2 mg L-1 and 5423,1 mg L-1, respectively. It has been observed that the susceptibility to localized corrosion was lower in the culture medium due to its lower chloride content. Fe was the most released metal in both media during the corrosion process. The concentrations were 0,570 mg L-1 in the NaCl aqueous solution and 0,480 mg L-1 in the culture medium. The concentrations of Cr and Mo released were similar in both media, having been 0,040 mg L-1 and 0,010 mg L-1, respectively, while Ni was only detected in the NaCl aqueous solution, 0,100 mg L-1. These concentrations of ions released did not cause cytotoxic effects in osteoblast-like cells.