Método de determinación en laboratorio de retención de creosota en muestras de eucaliptus impregnados
Método de determinación en laboratorio de retención de creosota en muestras de eucaliptus impregnados
cic.isFulltext | true | es |
cic.isPeerReviewed | true | es |
cic.lugarDesarrollo | Laboratorio de Entrenamiento Multidisciplinario para la Investigación Tecnológica | es |
cic.version | info:eu-repo/semantics/publishedVersion | es |
dc.date.accessioned | 2015-08-04T15:14:00Z | |
dc.date.available | 2015-08-04T15:14:00Z | |
dc.identifier.uri | https://digital.cic.gba.gob.ar/handle/11746/927 | |
dc.title | Método de determinación en laboratorio de retención de creosota en muestras de eucaliptus impregnados | es |
dc.type | Artículo | es |
dcterms.abstract | Se realizaron ensayos para determinar la retención de creosota en albura de eucaliptus viminalis y saligna, utilizando la Norma ASTM-D-1 860 y algunas variantes de la misma. Se concluye que: la desviación normal estimada de las determinaciones (precisión) es de aproximadamente 1 % la diferencia entre los resultados obtenidos en tres laboratorios (reproducibilidad) es de aproximadamente 1 % la diferencia entre los valores obtenidos sobre pastillas cortadas de tarugos de 15 mm de diámetro y 2 cm de largo, y valores obtenidos sobre muestras de astillas tomadas de los 2 cm de corona exterior de tortas cortadas de los mismos postes es de 16 %, con desviación normal de 2 % la diferencia entre los valores de retención obtenidos luego de 7-8 meses de impregnación y los valores originales es de aproximadamente 1 %. | es |
dcterms.abstract | A series of creosote retention tests on sapwood of eu- caliptus viminalis and e. saligna were performed by using the standard ASTM-D-1 860 and some varying of it. Conclusions are obtained as follows: the estimated standard deviation of the determinations (precision) is about 1 %; the difference detected between results obtained in three laboratories (reproducibility) is about 1 % the difference detected in values obtained on samples made up by tablets obtained from cores of 15 cm of diameter and of 2 cm lenght, and those* obtained from samples made up by chips taken off the outer 2 cm zone from 30 cm specimens cutted from the aforesaid poles is of 16 % with a standard deviation of 22 %; the difference between the retention values obtained after 6 or 8 months of impregnation and the original values, is about 1 %. | en |
dcterms.alternative | Laboratory determination method of creosote retention on impregnated eucaliptus samples | es |
dcterms.creator.author | Borlando, Luis | es |
dcterms.creator.author | Becka, Leopoldo | es |
dcterms.extent | p. 191-209 | es |
dcterms.isPartOf.issue | Serie II, 1973, nº 3 | es |
dcterms.isPartOf.series | Anales LEMIT | es |
dcterms.issued | 1973 | |
dcterms.language | Español | es |
dcterms.license | Attribution 4.0 International (BY 4.0) | es |
dcterms.publisher | Laboratorio de Entrenamiento Multidisciplinario para la Investigación Tecnológica (LEMIT) | es |
dcterms.subject | Eucaliptos | es |
dcterms.subject | Normas | es |
dcterms.subject | Retención | es |
dcterms.subject.materia | Ingeniería de los Materiales | es |
Archivos
Paquete original
1 - 1 de 1
- Nombre:
- 07-metodo de determinacion en laboratorio.pdf
- Tamaño:
- 688.39 KB
- Formato:
- Adobe Portable Document Format
- Descripción:
- Documento completo