Efecto de las variables del procedimiento de soldadura sobre las propiedades mecánicas y la resistencia a la corrosión en depósitos de soldadura de aceros inoxidables supermartensíticos
| cic.isFulltext | true | es |
| cic.isPeerReviewed | true | es |
| cic.lugarDesarrollo | Instituto de Investigaciones en Ingeniería Industrial | es |
| cic.parentType | Tesis | |
| cic.thesis.degree | Doctor de la Universidad de Buenos Aires. Área Ingeniería. | es |
| cic.thesis.grantor | Universidad de Buenos Aires | es |
| dc.date.accessioned | 2017-01-03T10:59:22Z | |
| dc.date.available | 2017-01-03T10:59:22Z | |
| dc.identifier.uri | https://digital.cic.gba.gob.ar/handle/11746/5116 | |
| dc.title | Efecto de las variables del procedimiento de soldadura sobre las propiedades mecánicas y la resistencia a la corrosión en depósitos de soldadura de aceros inoxidables supermartensíticos | es |
| dc.type | Tesis de doctorado | es |
| dcterms.abstract | Welding of martensitic stainless steels has presented some difficulties and the use of post weld heat treatments is usually required. The reasons are different for each grade of steel, but in general it is common to obtain high hardness and low toughness in the heat affected zone. This fact is associated with both martensitic structure and the carbon content. One possible solution to this problem and to achieve certain properties in as welded condition or after certain heat treatments, is both to reduce C content to very low levels which improves the weldability and decreases the hardness, and to add elements such as Mo and Cu to improve corrosion resistance and Ni to find the chemical balance between gamma and alpha phase stabilizer elements, trying to achieve a fully martensitic structure. These alloys solidify as ferrite delta. The transformation of delta ferrite to austenite begins at about 1300 ºC and ends, in the case of equilibrium conditions, at around 1200 ºC. With actual cooling rates during the welding process, small amounts of delta ferrite are retained in the microstructure, as well as varying amounts of austenite. These steels offer good resistance to corrosion in sweet or slightly acidic environments and applications have been developed for OCTG (oil country tubular goods). Since the mid 90's it is possible to weld this steels and their use has been increased almost exclusively in the gas and oil industry. The aim of this thesis was to study and understand the relationships among the variables of the welding process, the microstructure and the properties of all weld metal. In turn, it was looked for the optimum welding parameters to obtain microstructures that maximize these properties, providing additional information on the metallurgical characteristics of these deposits. The microstructural characteristics, mechanical properties, resistance to corrosion and hydrogen damage of a supermartensitic stainless steel deposit, were studied. The variables analyzed were the heat input, shielding gas and post weld heat treatment. This study was conducted on twelve all weld metal coupons welded in accordance with ANSI/AWS A5.22-95 with a metal cored wire of 1.2 mm diameter, deposited under semiautomatic metal cored arc welding process (MCAW). The different shielding gases used were: Ar+5%He, Ar+2%CO2 and Ar+18%CO2. The chemical composition was determined by optical emission spectrometry and the contents of C, O, N and S measured by Leco. The microstructural characterization was carried out using optical microscopy, SEM and X-ray diffraction determining, approximately, the content of delta ferrite and retained austenite in the deposits. The mechanical characterization was performed by hardness measurements, tensile test and Charpy-V impact test. With some samples complementary lines were developed: short-time heat treatments, maximizing the toughness, stability of austenite, pitting corrosion, stress corrosion cracking and hydrogen damage. In general, the contents of Cr, Ni, Mo, Si, Cu and Mn decreased slightly with increasing CO2 content in the shielding gas and contents of C, O and N increased. This was observed on the coupons welded with both high and low heat input. In all cases, the microstructure consisted of a martensitic matrix with small amounts of delta ferrite, retained austenite and some precipitates in as welded condition. The specimens welded with high CO2 content in the atmosphere presented, for the same heating rate (1 °C/min), higher temperatures AC1 and AC3. It was found a slight increase in hardness and tensile strength and decrease in toughness when increasing the content of CO2 in the shielding gas. The post weld heat treatment decreased slightly the hardness and tensile strength and improved toughness, reaching the best values, the specimens welded under Ar+He. The post weld heat treatment of solubilized + double tempering (1000 °C – 60 min + 650 °C – 15 minutes + 600 °C – 15 minutes) gave the highest values of retained austenite at room temperature. These microstructural conditions generated the highest values of impact toughness, increase 250 and 310 % toughness, compared with as weld conditions for samples welded with Ar+5%He and Ar+18%CO2, respectively. In the pitting corrosion tests, it was observed that the specimen in as welded condition provided a microstructure less susceptible to this corrosion mechanism regarding to heat treated specimen. A higher concentration of aggressive ions decreased the resistance to pitting corrosion. Precipitation phenomena associated with post weld heat treatments would control the corrosion resistance, as it was found intergranular stress corrosion cracking performed at 100 °C, 10 bars of CO2 in a solution with high Cl- content. The tensile strength decreased under hydrogen charging and the specimens with higher hardness values were the most susceptible to this type of damage. | en |
| dcterms.alternative | Effect of welding variables on mechanical properties and corrosion resistance of supermartensitic stainless steel weld metals | en |
| dcterms.contributor.director | De Vedia, Luis | es |
| dcterms.contributor.director | Svoboda, Hernán Gabriel | es |
| dcterms.contributor.director | Surian, Estela | es |
| dcterms.creator.author | Zappa, Sebastián | es |
| dcterms.extent | 384 p. | es |
| dcterms.issued | 2011-04-01 | |
| dcterms.language | Español | es |
| dcterms.license | Attribution-NonCommercial-NoDerivatives 4.0 International (BY-NC-ND 4.0) | es |
| dcterms.subject | Soldadura | es |
| dcterms.subject.materia | Ingenierías y Tecnologías | es |
Files
Original bundle
1 - 1 of 1
Loading...
- Name:
- Zappa, Sebastián - Tesis Doctoral.pdf-PDFA.pdf
- Size:
- 15.9 MB
- Format:
- Adobe Portable Document Format
- Description:
- Documento completo